AFFINITY™ PL 1880G
A polyolefin plastomer designed to offer low seal initiation temperature and good hot-tack strength for excellent packaging hermeticity at high packaging speeds, excellent seal through contamination and the possibility to seal heat sensitive polyolefin laminates.
Overview
AFFINITY* PL 1880G Polyolefin Plastomer (POP) is produced via INSITE* Technology. It is designed for a variety of demanding packaging applications, including high-speed form-fill-seal packaging.
This resin offers excellent ultimate hot tack strenath and low temperature seal initiaton, even through contamination in the package.
- Low seal initiation temperature
- Excellent hot tack strength
- High performance sealant layer in flexible packaging
Complies with:
- U.S. FDA FCN 424
- U.S.FDA-DMF
- U.S. USP 23
- HPFB No Objection (with limitations)
- EU, No 10/2011.
- Japan Hygienic Olefin and Styrene lastics Association
Consult the regulations for complete details.
Additive
- Antiblock: No
- Slip: No
- Processing Aid: No
Properties
| Nominal Value(English) | Nominal Value(SI) | Test Method | ||
| Physical | Density | 0.902 g/cm3 | 0.902 g/cm3 | ASTM D792 |
| Melt index (190℃/2.16kg) | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 | |
| Films | Film Thickness – Tested | 2.0 mil | 51 μm | |
| Film Puncture Energy (2.0 mil(51 μm)) | 78.0 in · lb | 8.81 J | Dow Method | |
| Film Puncture Force (2.0 mil(51 μm)) | 20.8 lbf | 92.5 N | Dow Method | |
| Film Puncture Resistance (2.0 mil(51 μm)) | 270 ft · b/in3 | 22.3 J/cm3 | Dow Method | |
| Secant Modulus
2% Secant, MD : 2.0 mil (51 μm) 2% Secant, TD : 2.0 mil (51 μm) |
13300 psi
13400 psi |
91.7 MPa
92.4 MPa |
ASTM D882 | |
| Tensile Strength
MD: Yield, 2.0 mil (51 μm) TD: Yield, 2.0 mil (51 μm) MD: Break, 2.0 mil (51 μm) TD: Break, 2.0 mil (51 μm) |
1050 psi
1000 psi 8500 psi 6480 psi |
7.24 MPa
6.89 MPa 58.6 MPa 44.7MPa |
ASTM D882 | |
| Tensile Elongation
MD: Break, 2.0 mil (51 μm) TD: Break, 2.0 mil (51 μm) |
620 %
630 % |
620 %
630 % |
ASTM D882 | |
| Dart Drop Impact 2.0 mil (51 μm) | > 830 g | > 830 g | ASTM D1709B | |
| Elmendorf Tear Strength1
MD : 2.0 mil (51 μm) TD : 2.0 mil (51 μm) |
550 g
720 g |
550 g
720 g |
ASTM D1922 | |
| Seal Initiation Temperature2
2.0 mil (51 μm) |
185 ℉ | 85.0 ℃ | Dow Method | |
| Thermal | Vicat Softening Temperature | 187 ℉ | 86.0 ℃ | ASTM D1525 |
| Melting Temperature (DSC) | 210 ℉ | 99.0 ℃ | Dow Method | |
| Optical | Gloss (20℃, 2.00 mil (50.8 μm)) | 141 | 141 | ASTM D2457 |
| Clarity (2.00 mil (50.8 μm)) | 83.0 | 83.0 | ASTM D1746 | |
| Haze (2.00 mil (50.8 μm)) | 1.10 % | 1.10 % | ASTM D1003 | |
| Extrusion | Melt Temperature | 408 ℉ | 209 ℃ | |
| Extrusion Nptes | Fabrication Conditions For Blown Film
|
|||
Notes
These are typical properties only and are not to be construed as specifications. Users should confim results by their own tests.
1Modified rectangular test specimen.
2Temperature at which 2 lb/in. (8.8 N/25.4 mm) heat seal strength is achieved.
Heat Seal Strengths, Topwave HT Tester 0.5 S dwell, 40 psi bar pressure, pull speed 10 in./min (250 mm/sec).
Parameters
| Minimum Order Quantity: | 25kg |
| Price: | $1.8-$3.2 |
| Packaging Details: | 25kg/bag |
| Delivery Time: | 3-5 working days to departure port |
| Payment Terms: | TT/LC |
| Supply Ability: | 1000MT/Month |